Formation and microscopic textures of Portland cement clinker minerals. Part 2
 
 
More details
Hide details
 
Publication date: 2006-05-01
 
 
Cement Wapno Beton 11(3) 135-158 (2006)
 
 
REFERENCES (26)
1.
K. Fukuda, I. Maki: Orientation of β-Ca2SiO4 Solid Solution Lamellae Formed in the Host -Phase, Cem. Concr. Res., 19[6] 913-918(1989).
 
2.
K. Fukuda, I. Maki: Remelting Reaction within Belite Crystals during Cooling, J. Am. Ceram. Soc., 75[10] 2896-98(1992).
 
3.
K. Fukuda, I. Maki, S. Ikeda, S. Ito: Microtextures Formed by the Remelting Reaction in Belite Crystals, J. Am. Ceram. Soc., 76[11] 2942-44(1993).
 
4.
I. Maki, K. Fukuda, T. Imura, S. Ito: Formation of Belite Clusters from Quartz Grains in Portland Cement Clinker, Cem. Concr. Res., 25[4] 835-840(1995).
 
5.
I. Maki, K. Masaki: Phase Composition and Morphology Change of the Clinker Constituent Minerals with Prolonged Heating at Elevated Temperatures, Proc. 20th Int. Conf. Cement Microscopy, pp.48-54, Guadalajara, Mexico, 1998.
 
6.
I. Maki, K. Masaki: Effect of Prolonged Heating at Elevated Temperatures on the Phase Composition and Textures of Portland Cement Clinker, Cem. Concr. Res., 32 931-934(2002).
 
7.
I. Maki: Nature of the Prismatic Dark Interstitial Material in Portland Cement Clinker, Cem. Concr. Res., 3[3] 295-313(1973).
 
8.
I. Maki, A. Ito: An Orthorhombic C3A Series Containing a Small Amount of SiO2 in Solid Solution, Semento Gijutu Nenpo 25, 18-22(1971); CAJ Review of the 25th General Meeting 1971, pp.23-25.
 
9.
I. Maki: Morphology of the So-called Prismatic Phase in Portland Cement Clinker, Cem. Concr. Res., 4[1] 87-97(1974).
 
10.
I. Maki: Optical Properties of the Anisotropic C3A, Cem. Concr. Res., 6[2] 183-192(1976).
 
11.
I. Maki: Optics and Phase Relationships of the Optically Anisotropic C3A, Cem. Concr. Res., 6[6] 797-802(1976).
 
12.
R. Kondo, S. Choi: Mechanism and Kinetics of Portland Cement Clinker Formation for an Example of the Solid State Reaction in the Presence of a Liquid Phase, Proc. 5th Int. Conf. Chem. Cement, Vol. 1, pp.163-171 ,Tokyo, 1968.
 
13.
I. Maki, K. Fukuda, E. Oba, H. Yoshida, M. Mitsumatsu, S. Ito: Anisotropic Light Absorption of the Calcium Aluminoferrite Phase in Portland Cement Clinker, Cem. Concr. Res., 25[4] 863-869(1995).
 
14.
I. Maki, M. Ichikawa, H. Yoshida, T. Yoshida: Anisotropic Light Absorption of the Ferrite Solid Solutions Ca2(Fe1-xAlx)2O5, Cem. Concr. Res., 26[12] 1801-1808(1996).
 
15.
Y.M. Butt, V.V. Timashev: The Mechanism of Clinker Formation. Processes and Ways of Modifi cation of Clinker Structure (Principal Paper), p.52, 6th Int. Symp. Chem. Cement, Moscow, 1974.
 
16.
V.V. Timashev: The Kinetics of Clinker Formation. The Structure and Composition of Clinker and its Phases, Proc. 7th Int. Symp. Chem. Cement, I-3/1-20, Paris, 1980.
 
17.
I. Maki: Mechanism of Glass Formation in Portland Cement Clinker, Cem. Concr. Res., 9[6] 757-763(1979).
 
18.
S. Takashima, K. Higaki: Dissolution and Determination of Glass Phase in Portland Cement by the Picric Acid Methanol Method, Semento Gijutu Nenpo 23, 35-38(1969); CAJ Review of the 23rd General Meeting 1969, pp.47-50.
 
19.
M. Regourd, A. Guinier: The Crystal Chemistry of the Constituents of Portland Ce-ment Clinker (Principal Paper), p.47, 6th Int. Symp. Chem. Cement, Moscow, 1947.
 
20.
J.A. Imlach: Nonisothermal Investigation of the Kinetics of Reactions Occurring during Clinker Formation, Cem. Concr. Res., 6[6] 747-755(1976).
 
21.
S. Chromý, I. Maki: Infl uence of Heating Rates on the Kinetics of Portland Clinker Formation, Il Cemento, 88[1] 19-28(1991).
 
22.
I. Maki, H. Kamei, M. Nakura, Y. Mizuno: Kinetics of Formation and Fine Textures of Alite in Portland Cement Clinker, Proc. 17th Int. Conf. Cement Microscopy, pp.61-70, Calgary, Alberta, Canada, 1995.
 
23.
J.A. Chesley, G. Burnet: A Two-Stage Reaction Sequence for C3S Formation, Cem. Concr. Res., 19[6]837-847(1989).
 
24.
I. Maki, T. Tanioka, T. Hibino: Formation of Portland Clinker Nodules in Rotary Kilns and Fine Textures of Constituent Phases, Il Cement, 86[1] 3-10(1989).
 
25.
I. Maki, K. Masaki, M. Suzuki: Burning and Nodulization Process of Clinker in the Rotary Kiln As Viewed from the Fine Textures of the Constituent Minerals, Proc. 6th Euroseminar on Microscopy Applied to Building Materials, pp.32-40,.Reykjavik, Iceland, June 25-27, 1997; K. Masaki, M. Suzuki, I. Maki: Cem. Concr. Res., 32, 1039-1044 (2002).
 
26.
I. Maki, T. Tanioka, S. Ito, K. Maeda, K. Fukuda: Texture and Grindability of the Dust Component in Portland Cement Clinker, Cem. Concr. Res., 24[3] 497-502 (1994).
 