Effect of chloride salt and freeze-thaw cycling on the microstructure of concrete
Min Li 1,2
,
 
,
 
,
 
 
 
 
More details
Hide details
1
Jiangsu Key Laboratory for Construction Materials, Southeast University, Nanjing, China
 
2
International Institute for Urban System Engineering, Southeast University, Nanjing, China
 
 
Publication date: 2013-03-01
 
 
Cement Wapno Beton 18(2) 74-80 (2013)
 
KEYWORDS
ACKNOWLEDGEMENTS
The authors gratefully acknowledge the fi nancial support for this research from the Major State Basic Research Development Program of China (973 Program) (2009CB623203) and Program for New Century Excellent Talents in University of Ministry of education of China(NCET-11-0091)
 
REFERENCES (16)
1.
Tamon UEDA. Durability design concept in Asian Concrete Model Code and its future direction.Hokkaido University Japan 2005.10.
 
2.
Z. H. Sun, George W. Scherer, Effect of air voids on salt scaling and internal freezing, Cem.Concr. Res., 40, 260–270 (2010).
 
3.
S. Y. Huang, J. F. Jiang, Modern concrete technology, ShanXi science and technology press 1988.
 
4.
Veas Penttala, Fahim Al-Neshawy, Stress and strain state of concrete during freezing and thawing cycles, Cem. Concr. Res. 32, 1407–1420 (2002).
 
5.
T. C. Powers, A Working Hypothesis for Further Studies of Frost Resistance of Concrete, RX005, Portland Cement Association, 245-272, Chicago 1945.
 
6.
T. C. Powers, The Air Requirement of Frost-Resistant Concrete, Proceedings of the Highway Research Board, Portland Cement Association, Bulletin, 33, 1-8 (1949).
 
7.
T. C. Powers, T. L. Brownyard, „Studies of the Physical Properties of Hardened Portland Cement Paste. IV. The Thermodynamics of Adsorption of Water on Hardened Paste,” Journal of the American Concrete Institute 18, 549-602 (1947).
 
8.
T. C. Powers, R. A. Helmuth, Theory of Volume Changes in Hardened Portland Cement Paste During Freezing, Proceedings of the Highway Research Board, 32, 285 (1953).
 
9.
G. Fag erlund, The critical degree of saturation method of assessing the freeze-thaw resistance of concrete. Materials And Structures 10, 217 – 229 (1977).
 
10.
Andrzej Cwirzen, Aggregate–cement paste transition zone properties affecting the salt–frost damage of high-performance concretes. Cem. Concr. Res. 35, 671–679 (2005).
 
11.
Vesa Penttala, Surface and internal deterioration of concrete due to saline and non-saline freeze–thaw loads, Cem. Concr. Res. 36, 921 – 928 (2006).
 
12.
Olivier Coussy, Paulo J. M. Monteiro, Poroelastic model for concrete exposed to freezing temperatures, Cem. Concr. Res. 38, 40–48 (2008).
 
13.
Mahmoud Nili, Deicer salt-scaling resistance of non-air-entrained rollercompacted concrete pavements, Constr. Build. Mat. 25, 1671–1676 (2011).
 
14.
China Academy of Building Research, Standard for test method of longterm properties and durability of ordinary concrete(GBJ82-- 85), BeiJing, Standards Press of China, 2005.12.
 
15.
R. Mu, Durability and Service Life Prediction of Concrete Subjected to the Combined Action of Freezing-Thawing, Sustained External Flexural Stress and Salt Solution, Southeast university Ph.D. Dissertation, NanJing 2000.
 
16.
Z. W. Wu, L. H. Lian: High Performance Concrete[M]. BeiJing, Atomic Energy Press 2000.
 
ISSN:1425-8129
Journals System - logo
Scroll to top